Under steel standard DIN 17102,there are four different grades for 355 Mpa steel,StE355,WStE355,TStE355 and EStE355.These four structural steel grades contains the same chemical composition for cast analysis except a little difference in Carbon contains,also owned the same yield strength and tensile strength values range.Xinsteel supply low alloy steel plate under steel standard EN,DIN,BS,GB,ASTM,ASME AND JIS which including many steel grades we can offer.


Get an valued quotation for TStE355 structural steel plate,NOW CONTACT XINSTEEL.


Other relative low alloy steel grades under steel standard EN 10025 S275JR steel plate,S355JR plate steel,S275J0 structural steel plate,S355J0 low alloy steel plate,S275J2 steel plate,S355J2 plate steel,S355K2 structural steel plate,S450J0 low alloy steel plate, S275M steel plate,S275ML plate steel,S355M structural steel plate,S420M low alloy steel plate, S460M steel plate,S355ML plate steel,S460ML structural steel plate,S420ML low alloy steel plate.Din17102 steel specification has StE420 steel plate,WStE420 plate steel,TstE420 structural steel plate,EstE420 low alloy steel plate, StE460 steel plate,WStE460 plate steel,TstE460 structural steel plate,EstE460 low alloy steel plate, StE500 steel plate,WStE500 plate steel,TstE500 structural steel plate,EstE500 low alloy steel plate. JIS G3106 steel standard contains SM490A steel plate,SM490B steel sheet,SM490C structural steel plate,SM490YA steel plate,SM490YB low alloy steel plate,sm520b steel,SM520C steel plate,sm570 plate steel.


Chemical composition of Cast analysis for TStE355 structural steel plate (Max %)

 

TStE355

Steel Plate

C

Si

Mn

P

S

N

0.18

0.10/0.50

0.90/

1.65

0.030

0.025

0.020

Cr

Cu

Mo

Ni

V

Nb+Ti+V

0.30

0.20

0.08

0.30

0.10

0.12