HEM steel beam also called as IPBV steel beam,this beam is heavy section with thick flange and heavy unit weight comparing with HEA steel beam and HEB steel beam.In specification EN 10025-2,there are low temperature steel materials of S275J0 HEM Steel Beam and S275J2 HEM Steel Beam.These steel beams both owned minimum yield strength as 275 Mpa.Stock sizes for S275J0 steel beam and S275J2 steel beam heavy sections as HEM100 H120*106*12*20
HEM120 H140*126*12.5*21HEM140 H160*146*13*22 HEM160 H180*166*14*23 HEM180 H200*186*14.5*24
HEM200 H220*206*15*25 HEM220 H240*226*15.5*26 HEM240 H270*248*18*32HEM260 H290*268*18*32.5
HEM280 H310*288*18.5*33 HEM300 H340*310*21*39 HEM320 H359*309*21*40 HEM340 H377*309*21*40


Besides HEM steel beams,we also stock for low temperature S275J0 steel plate,S275J2 steel plate,S275J0H seamless steel pipe,S275J2 welded steel pipe,S275J0H hollow sections,S275J2H square hollow sections with traceabe mill test certificates.


Comparasion with S275J2 HEM steel beam and S275J2 HEM steel beam in chemical composition and mechanical property:

 

S275J2 vs S275J0

Chemical composition: Heat Analysis  Max%

Standard

Grade

C

Mn

P

S

Si

N

Cu

EN 10025-2

S275J0

0.18

1.50

0.030

0.030

-

0.012

0.55

EN 10025-2

S275J2

0.18

1.50

0.025

0.025

-

-

0.55

Mechanical Properties:

Thickness

Yield strength

Tensile strength

Mpa  Min.

Mpa

EN 10025-2

S275J0

3<T≤16

275

410-560

EN 10025-2

S275J2

3<T≤16

275

410-560