High strength shipbuilding steel angle LR Grade AH32 is owned higher steel strength at minimum yield strength 315 Mpa and with minimum tensile strength 440 Mpa.Done low temperature impacting test for LR Grade AH32 under zero centigree when rolling.For angle steel LR Grade AH32,xinsteel roll type equal angle steel LR Grade AH32,unequal angle steel LR Grade AH32 and unequal leg and unequal thickness angle steel LR Grade AH32.


Our high quality angle steel for shipbuilding have been approved by nine classification societies,besides LR Grade AH32 shipbuilding steel angles,we can roll ABS Grade AH32 shipbuilding angle steel,DNV Grade AH32 shipbuilding angle steel,BV Grade AH32 angle steel,GL Grade AH32 steel angle for ship,KR Grade AH32 steel angle,NK Grade AH32 ship angle steel,CCS Grade AH32 and RINA Grade AH32 shipbuilding steel angles.

 

Chemical composition of Heat analysis for Shipbuilding angle steel LR Grade AH32 (Max %):

C

Mn

Si

P

S

Al

(acid)

Nb

0.18

0.90-1.60

0.50

0.035

0.035

≥ 0.015

0.02-0.05

Ti

V

Ni

Cu

Cr

Mo

0.02

0.03--0.10

0.40

0.35

0.20

0.08