ABS FH36 ship plate and DNV EH36 ship plate owned minimum yield strength at 355 Mpa and tensile strength within 490 to 620 Mpa.In chemical composition,ABS FH36 contains V% as 0.03-0.10% and DNV EH36 contains V% as 0.05-0.10%.
ABS FH36 steel plate and DNV EH36 steel plate are both high tensile strength steel materials for marine hull structural usage.DNV EH36 also called as DNV-GL EH36 or VL EH36.ABS FH36 ship plate done low temperature impacting test at -60 Deg.Centigrade and ABS EH36 ship plate done low temperature impacting test at -40 Deg.Centigrade.Shipbuilding steel materials ABS A,ABS AH36 bulb flat,ABS AH36 angle bar,VL AH36 steel plate,VL AH32 steel angle,LR A steel plate,LR A steel angle are in our stock warehouse.
Comparasion of ABS FH36 ship plate and DNV EH36 ship plate steel properties:
ABS FH36 vs DNV EH36 |
Chemical composition: Heat Analysis Max% | |||||||||
Standard |
Grade |
C |
Mn |
P |
S |
Si |
Cr |
Cu |
Nb |
V |
ABS |
FH36 |
0.16 |
0.9-1.6 |
0.025 |
0.025 |
0.5 |
0.20 |
0.35 |
0.02-0.05 |
0.03-0.10 |
DNV |
EH36 |
0.18 |
0.9-1.6 |
0.035 |
0.035 |
0.1-0.5 |
0.20 |
0.35 |
0.02-0.05 |
0.05-0.10 |
Mechanical Properties: |
Yield strength |
Tensile strength | ||||||||
Mpa Min. |
Mpa | |||||||||
ABS |
FH36 |
355 |
490-620 | |||||||
DNV |
EH36 |
355 |
490-620 |